Dear Experts, 

As per ASME IX 

QW-304 Welders :

Except for the special requirements of QW-380, each  welder who welds under the rules of the Code shall have  passed the mechanical and visual examinations prescribed
in QW-302.1 and QW-302.4 respectively. Alternatively, welders making a groove weld using SMAW, SAW, GTAW, PAW, and GMAW (except short-circuiting mode)
or a combination of these processes, may be qualified by radiographic examination,

WHY SHORT- CIRCUITING MODE IS EXCEPTIONAL  ??? 

Regards.

Abhishek Ghosh 

--
ABHISHEK GHOSH
FAHAHEEL, KUWAIT
MOB: (00)965-60303798

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...