Dear Joshi,

 

I did not read your document properly, I just saw that you specify 110 MPa at a temperature of 380 °C but this 110 MPa is maximum allowed at 400 °C for thickness up to 50 mm. For your thickness of 75 mm max allowed is 100 MPa at 400 °C. I don’t have any experience with how to calculate values allowed for temperatures between 350 °C and 400 °C. Still hope the copy below will help you further.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: Pieper QSI [mailto:pieper-qsi@kpnmail.nl]
Verzonden: dinsdag 24 mei 2011 20:41
Aan: 'materials-welding@googlegroups.com'
Onderwerp: RE: 11134] DIN - K-value of Flange

 

Dear Joshi,

 

Please find below a part of table 6 of specification EN 10273 which replaces the mentioned DIN 17243 specification.

You can see that the “Werkstoff nummer” of the material P250GH is similar to the number of C22.8, both 1.0460 so this is the same material but only according to the new European standard, the DIN specification is withdrawn so I can’t find/give you a copy of that.

As you can see you can calculate with values up to 237 MPa at 100°C depending on material thickness.

I hope this will help you out.

 

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Joshi
Verzonden: dinsdag 24 mei 2011 9:58
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:11134] DIN - K-value of Flange

 

Dear Friends,

 

I attach here the Design calculation of flanges done by our consultant according to AD-Merkblatter. The flange rating is PN-40. The DIN Flange material is C22.8 DIN 17243 AD-W12/W13 , WERKSTOFF NUMBER IS 1.0460. According to Table of Material Equivalent Chart as reference , The equivalent material of this flange is A105N. 

 

The client want us to confirm the validity of the K-value given in the calculation at the designated temperature. I don't have any reference cannot find the list of K-VALUE d list for the flange to check on its value. If using PVElite and ASME Sect VIII Div 1, For Flange of A105 , the design stress value at 100 Degree C. will be at 120 N/mm3. Can I use that and show it to the client?.

 

 

 




***DISCLAIMER NOTICE: ***

"The information contained in this email and/or any attachment hereto is strictly confidential and privileged. If you are not the intended recipient, and/or have received this email in error, you must not copy, disseminate or disclose the contents of this message and/or any attachment to any other person. Please notify the sender and delete this message and any attachment from your system. KNM accepts no liability in respect of prohibited and unauthorised use by an unintended addressee or recipient. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group. Although this email and/or any attachment is believed to be free of any virus or other defect which may affect any computer system into which it is received and opened, it is the responsibility of the recipient to ensure that it is virus-free and KNM accepts no responsibility for any loss or damage arising in any way from the use thereof."


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...