Sunday, May 29, 2011

Re: [MW:11192] Any idea of Twin Tig welding of Duplex steel

For Duplex SS , no autogenous welding ( only Fusing will affect Phase balance)

On Sat, May 28, 2011 at 10:27 PM, mohd Dohad <mohd52100@gmail.com> wrote:
Our client tell us to do twin tig welding for duplex steel 31803 to
reduce distortion.does anybody has experieced how could this welding
is performed?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...