RE: [MW:11211] ARC Blow

In general The shifting of the arc in various directions in electric-arc welding due to the magnetic fields at the arc.

OR

A welding arc may be deflected away from the point of welding, which can mean that the weld quality may suffer. Such arc deflection, usually forward or backward of the welding direction, is known as 'arc blow'.

 

Arc blow tends to occur if the material being welded has residual magnetism at a certain level, particularly when the weld root is being made. This is due to interaction between the directional magnetic field of the welding arc and the directional field of the residual magnetism.

 

Remedies for Arc Blow - Arc blow can be minimized by keeping the following factors in view:

1. Electrode geometry in non consumable electrode welding (e.g., TIG and carbon arc welding).

2. Changing the position of earth clamp or current return lead and welding away from the earth connection.

3. Avoiding the presence of (or rearranging) magnetic materials around the workpiece and arc.

4. Storing workpieces away from magnetic sources, such as welding power sources.

5. Lowering the arc current.

 

ETC

 

Thanks

 

 

 

Regards,

Prakash Verma

Aker Drilling Risers

Aker Solutions

MOBILE - 0047-40466591

DESK- 0047-22945932

Email: Prakash.Verma@akersolutions.com

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of we1414
Sent: 30. mai 2011 11:26
To: Materials & Welding
Subject: [MW:11206] ARC Blow

 

Dear experts Hello to all of you as i m new to this group.

my query is about arc blow. pleas explain why it occurs during welding

and how can it be controlled.

 

--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 


This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...