Tuesday, May 24, 2011

Re: [MW:11132] Re : Gas use for Backing and Purging

Hi,
Argon-99.95% purity is good for Duplex Welding.Backing gas shall also Pure Argon.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 5/24/11, mustaffi <mustaffi@dynac.com.my> wrote:

From: mustaffi <mustaffi@dynac.com.my>
Subject: [MW:11130] Re : Gas use for Backing and Purging
To: materials-welding@googlegroups.com
Date: Tuesday, May 24, 2011, 12:46 PM

Hi All

 

Can anybody can tell me, what it's the best gases to proceed welds for TIG process on Duplex Steel Material

 

Regards

Mus

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...