Dear Hafiz,
 
Steam blowing will be done generally to clean the steam piping before put the steam piping into service this will remove all loose mill scale, rust and foreign materials from piping. If left uncleaned, these particles will reach steam turbine blades through piping and damage them. Used for steam piping and steam circuits of boilers - power plants
 
Nitrogen purging is charging the piping with nitrogen gas before charging the line with hydro carbons/chemicals to make them inert (to displace the atmospheric air which contains oxgen) to avoid any explosion/chemical reaction. Used for hydrocarbon piping, pressure vessels, equipment etc. - oil and gas

Regards,
T.V.Ramakrishna.
On Sun, May 29, 2011 at 3:33 PM, Hafiz Ali Alvi <alimalvi300@hotmail.com> wrote:
Hello All,
 
My question is about difference between Blowing (e.g Steam Blowing) and Purging (e.g Nitrogen Purging). What is the main difference between these two operations and for what service we use it.
 
Regards.
 
Hafiz Ali Alvi
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...