Hi Abhishek,

 

GMAW Process short circuit have a tendency to give LOF.LOF is hard to find during RT.Mech. Testing Side bend testing opens up a LOF:

Hope this will help you out.

 

Thanks

Regards,
Prakash Verma

Aker Drilling Risers
Aker Solutions
MOBILE - 0047-40466591
DESK- 0047-22945932
Email: Prakash.Verma@akersolutions.com


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of John Henning
Sent: 25. mai 2011 17:45
To: materials-welding@googlegroups.com
Subject: [MW:11144] RE: 11128] QW 304: Welders

 

Short-circuiting mode GMAW receives special treatment because it has a history of welds being made with small, tight  lack of fusion defects both at the side wall and between weld beads/layers.  These are typically not detectable by RT but will open up when bend tested.  These defects are the result of weldor technique.  Understand that RT is an exemption/or permitted substitution for the required bend testing  In this case the use of RT as an exemption/substitution is not extended to the GMAW-S process.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ABHISHEK GHOSH
Sent: Monday, May 23, 2011 3:17 PM
To: materials-welding@googlegroups.com
Subject: [MW:11128] QW 304: Welders

 

Dear Experts, 

 

As per ASME IX 

 

QW-304 Welders :

 

Except for the special requirements of QW-380, each  welder who welds under the rules of the Code shall have  passed the mechanical and visual examinations prescribed

in QW-302.1 and QW-302.4 respectively. Alternatively, welders making a groove weld using SMAW, SAW, GTAW, PAW, and GMAW (except short-circuiting mode)

or a combination of these processes, may be qualified by radiographic examination,

 

WHY SHORT- CIRCUITING MODE IS EXCEPTIONAL  ??? 

 

Regards.

 

Abhishek Ghosh 


--

ABHISHEK GHOSH
FAHAHEEL, KUWAIT
MOB: (00)965-60303798

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...