we recently qualified for this material EN 10025-2-S355JR/EN10028-2 Gr
P355GH with E7018.its giving good result.we used for our structure
project.
On May 27, 6:28 am, kalyan vvv <vvvka...@gmail.com> wrote:
> Resp all,
> we established procedure for S355 JR with E7018 in SMAW
> process. It meets all the mechanical requirements.
> E7018 Electrode is sufficient for welding of S355 JR material
> in SMAW process.(Actually this material is european standard material there
> is no
> exactly equivalent material in ASTM)
> So It is better to use E7018 electrode.
> --
> *THANKS & REGARDS*
> * *
> *KALYAN VVV*
> *WELDING ENGINEER *
> *THYSSEN KRUPP INDUSTRIES (INDIA) LTD
> HYDERABAD
> *
> *Mob.NO- 09885273257*
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.