RE: [MW:6197] why we are not doing positive material identification in carbon steel materials

Dear all,

 

In these cases, when you need to quantify C, S, P, Mn, and Si then you need to use PMI technique utilizing the portable optical emission spectrometer. Arcmet 8000 which we have is a good equipment to undertake such tests at site in a non destructive manner.

 

Regards,

Rohit Bafna

Director - Global Sales

 

------------------------------------------

TCR Engineering Services (India)
TCR Arabia (KSA), TCR Kuwait

TCR Consulting FZC (UAE)

TCR Africa (RSA)

TCR World Inc. (USA)

Tel: +91-983-353-0400

www.tcreng.com
Material Testing | Consulting | Inspection | NDT Services

-------------------------------------------

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Manish.Maheta@Linde-LE.com
Sent: Thursday, July 29, 2010 11:02 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6195] why we are not doing positive material identification in carbon steel materials

 


 Carbon, Silicon, Sulfur, and Phosphorous are very light elements and it is not possible to quantify such as elements by performing PMI.
  Jigneshbhai ,your concurrence is requested for subject matter.

Regards,
Manish


rao <amma0509@gmail.com>
Sent by: materials-welding@googlegroups.com

29/07/10 22:10

Please respond to
materials-welding@googlegroups.com

To

"Materials & Welding" <materials-welding@googlegroups.com>

cc

Subject

[MW:6193] why we are not doing positive material identification in         carbon steel materials

 




dear sir
why we are not doing positive material identification in carbon steel
materials
please explain it

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...