Friday, July 30, 2010

Re: [MW:6195] why we are not doing positive material identification in carbon steel materials


 Carbon, Silicon, Sulfur, and Phosphorous are very light elements and it is not possible to quantify such as elements by performing PMI.
  Jigneshbhai ,your concurrence is requested for subject matter.

Regards,
Manish



rao <amma0509@gmail.com>
Sent by: materials-welding@googlegroups.com

29/07/10 22:10

Please respond to
materials-welding@googlegroups.com

To
"Materials & Welding" <materials-welding@googlegroups.com>
cc
Subject
[MW:6193] why we are not doing positive material identification in         carbon steel materials





dear sir
why we are not doing positive material identification in carbon steel
materials
please explain it

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...