Re: [MW:6185] Mo and Cr content exceeded in 15Mo3 material-reg

Those two elements are increasing hardness and reduce ductility so on my opinion you should reject them


  From: Karthik [karthik6684@yahoo.com]
  Sent: 28/07/2010 23:42 MST
  To: materials-welding@googlegroups.com
  Subject: [MW:6183] Mo and Cr content exceeded in 15Mo3 material-reg



Dear All,

We have received PMI report from our material supplier for 15Mo3 elbow before delivery.We found that Mo and Cr.Contents are higher than the maximum requirement.Please find below the details of Compositions.


Matrerial - 15Mo3

Standard Specification (Mo) = 0.25 to 0.35%

Actual found                (Mo) = 0.50%

Standard Specification (Cr) = 0.25 to 0.35%

Actual found                (Cr) = 0.90%


Shall we accept this material,since the Mo and Cr Percentage are exceeded.If it is acceptable,what will be the impact in the actual working conditions? (This material is used for Superheater)


Please give us your suggestion


Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...