RE: [MW:6184] Mo and Cr content exceeded in 15Mo3 material-reg

Generally a variation of 10% can be accepted in PMI, you can check the sample by other method. What MTC shows?
Investigate vendor might have supplied 1Cr 0.5Mo grade instead of 15Mo3, which require different tretment interms welding, PWHT etc.
sent from my handheld
-----Original Message-----
From: Karthik
Sent: 29/07/2010 12:12:27 pm
Subject: [MW:6183] Mo and Cr content exceeded in 15Mo3 material-reg


Dear All,We have received PMI report from our material supplier for 15Mo3 elbow before delivery.We found that Mo and Cr.Contents are higher than the maximum requirement.Please find below the details of Compositions.
Matrerial - 15Mo3Standard Specification (Mo) = 0.25 to 0.35%Actual found                (Mo) = 0.50%Standard Specification (Cr) = 0.25 to 0.35%Actual found                (Cr) = 0.90%
Shall we accept this material,since the Mo and Cr Percentage are exceeded.If it is acceptable,what will be the impact in the actual working conditions? (This material is used for Superheater)
Please give us your suggestion
Karthikeyan.S   Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...