Re: [MW:6156] Fail on Tensile Test

the reason may be the following items:
1-the surface of sample may be rough and stress concentration is occured.
2-depend of configuration of partial joint& used H.I in this PQR,previouse weld,the length of coarse grain area in HAZ may be larg.
3-due to concentrated impurities in haz.
item 2& 3 is clear with micro etch.

On Wed, Jul 28, 2010 at 5:52 AM, <candice@chopkiatsiang.com.my> wrote:
All,
I'd carried out a Repair WPQT for 2"Sch160 ASTM A106 pipe. We are to carry
out through repair and partial repair. After the mechanical testing in the
lab, the result failed on tensile test on the base metal. I's rechecked
back on the mill certificate for the pipe but showing no discrepency on the
mechanical properties. Could someone advice on the cause of the failure in
tensile on base metal. Will it because of the heating?

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...