Re: [MW:6155] why plsama cutting in ss

because the speed of cutting& concentration of heat in plasma  is more than oxyacetelene cuttng, therefore cooling rate is most&  St.St isn't sentisized.

On Tue, Jul 27, 2010 at 6:10 PM, mijin <mathew.mijin@gmail.com> wrote:
why we are using plasma cutting in stainless steel instead of
oxyacetelene cuttng.please give me a reason...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...