Sunday, July 11, 2010
RE: [MW:5938] RE: 5920] EA 395/9
dear all
follow this link t o find details
http://www.elmics.ru/material/el/el0301_e.htm
QA/QC ENG: AMR SOLIMAN
PETROJET-EGYPT
> Subject: Re: [MW:5936] RE: 5920] EA 395/9
> To: materials-welding@googlegroups.com
> From: vdm@supertechservices.in
> Date: Sun, 11 Jul 2010 00:51:53 +0000
>
> Thanks John,
>
> Are these only manufactured in Russia? Any other manufacturer you know elsewhere?
>
> Regards
>
> VISHAL MEHTA
>
> SUPERTECH SERVICES LTD
>
> Sent on my BlackBerry® from Vodafone
>
> -----Original Message-----
> From: "John Henning" <jhenning@deltak.com>
> Sender: materials-welding@googlegroups.com
> Date: Fri, 9 Jul 2010 14:30:47
> To: <materials-welding@googlegroups.com>
> Reply-To: materials-welding@googlegroups.com
> Subject: [MW:5922] RE: 5920] EA 395/9
>
> Try the following - Russian electrodes intended for buttering
> applications for ferritic to austenitic stainless
>
> http://www.elmics.ru/material/el/el0301_e.htm
>
> http://www.mmk-metiz.ru/eng/content/prices/catalogue/viewdoc_n_en/206
>
> John
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Vishal Mehta
> Sent: Friday, July 09, 2010 12:42 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:5920] EA 395/9
>
> Hello,
>
> Can anyone give details of EA 395/9 grade electrode, with its
> composition?
>
> Also who are the manufacturers of this electrode and its availability in
> India.
>
> Thanks
>
> Regards
>
> VISHAL MEHTA
>
> SUPERTECH SERVICES LTD
>
> Sent on my BlackBerry(r) from Vodafone
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hotmail: Trusted email with Microsoft's powerful SPAM protection. Sign up now.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment