Saturday, July 31, 2010

[MW:6224] ASME PQR-WPS-Impact testing

Guys,
Could anyone inthis group clarify whether is it required to do Impact testing for welding repair procedure qualification.Normally we do Tensile,bend,.
Here for API 5L PSL1 pipes we have already WPS/PQR with out Impact,so is it acceptable as per ASME SEC.IX

REGARDS,
KK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...