Monday, July 26, 2010

[MW:6133] SAW Wire Test certificate review

Frnds,
Here i received one SAW Wire test certificate for ESAB OK AUTOROD 12.22L ,as per ASME SEC II Part c SFA 5.17 EM12K.

In the Test certificate they gave only Chemical Analysis of the wire .

Shall I accept the Test certificate or I have to ask for Mechanical Properties also.

Is it acceptable the Test certficate as it is.

Kindly guide,

thanks,
KK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...