Wednesday, July 14, 2010

[MW:5978] Ring Gasket: Soft iron gasket vs. low carbon steel gasket

As per ASME B16.20, for ring gasket material, Soft iron gasket as well as Low-carbon steel gasket are mentioned, see below table from ASME B16.20

 

 

Can anyone, guide me what is the difference between SOFT IRON gasket and LOW CARBON STEEL gasket. As far as I know, SOFT IRON is having carbon content less than 0.1% and hence it is nothing but low carbon steel only.

 

Request opinion from group members.

 

 

Best Regards,

Sunil Agrawal