Hi Gents,
As per API 1104, can the qualified heat input range be established as follows for GMAW process?
1. The minimum qualified heat input shall be the minimum heat input recorded during PQR -10%
2. The maximum qualified heat input shall be the maximum heat input recorded during PQR +10%
3. While for SMAW process, Maximum qualified heat input shall be the maximum recorded during PQR.
Pls I want more contribution for clarity of purpose.
Regards
Philip Taiye
Principal QA/QC Welding Engineer
(MIPs Quality Control)
DeltaAfrik Engineering Limited
2nd Floor, City Express Bank Building
Plot
Victoria Island,
Phone: +234-1-461-8508, +2341-461-6137 ext. 1257
Cell: +234-(0)-803-803-1396
Fax: +234-1-262-2418
e-mail: taiye.philip@worleyparsons.com
*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."
No comments:
Post a Comment