Hi,

 

Have the following question regarding weld metal deposition on PQR with combined GTAW & MMAW processes.

Have recorded both GTAW = 3.5mm & MMAW = 9.8mm onto PQR (QW-204b) but unsure of the ranges qualified

for both and should they be recorded on associated WPS.

 