Thursday, April 1, 2010

Re: [MW:4653] Multiple PQRs for Impact test requirement

Hi Mr. Ibrahim,

In ASME VIII, Div. 1, UW-16 (c), indicates reference to the figures UW-16.1 (d) and (e)
If your joint design as the one I attached, you may not use the PQR 40 mm thick, and this complies with QW-403.6

Kind regards.

Gustavo Mendoza.
QA/QC Inspector.
Venezuela
mar 31, 2010 12:23:07 PM, materials-welding@googlegroups.com wrote:

===========================================

 Hi Members, Please provide a solution for the following issue. Shell Material : SA 516 Gr.70 -- 50 mm ThkNozzle : SA 333 Gr.6 --- 7 mm thk MDMT : - 46 Deg.C I need to weld the nozzle to shell. I have a PQR with SMAW process qualified in 40 mm thk and another PQR with SMAW qualified in 6 mm thk. As per Sec. IX if impact test is required the 40 mm PQR will support from 16 mm to 200 mm. base metal Thk. and the other PQR will support from 6 mm to 12 mm thk. If I club these PQR can I write a WPS to support 6 mm to 200 mm?.Is there any issue for the missing range of qualification between 12 mm to 16 mm?. Or is it required to add another PQR to fill the missing thickness range from 12 to 16 mm between the first two PQRs?.Or can I write a WPS directly with range 5mm to 200mm omiting impact test requirement for this joint as it is a category D joint and excempted from Production Test Coupon?.
Thanks & Regards
Muhammed Ibrahim PK


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe, reply using "remove me" as the subject.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...