Hi,
     First of all You have clearly indicate the material spec and product form ,Design code .
As per ASME B 31.3 you can use upto -425 Deg F(253.8 Deg C)  provided the material is solution annealed condition. Considering the welding the material can be used upto 101Deg F without Impact testing.
 
Regards,
Vaithiyanathan

On Tue, Apr 27, 2010 at 3:51 PM, KASHKOUSHA <kashkousha1@yahoo.com> wrote:
dear all
pls. what is the lowest temperature service for s.st 316l
pls ur refernce
thanks
 
H.KASHKOUSHA


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...