Hi Sasa,

 

Attached are  some guidelines on electrode selection and for welding of cast iron. Cast irons (SG and grey CIs) are weldable to a certain degree, white cast irons are not weldable. The conventional ways are to use Pure Nickel (99% ENi-CI) or Iron Nickel(55% Ni, E-NiFE-CI) electrodes. The later is more suited for welding on rusty, oiled and greased surfaces.

 

Cast iron could be inspected by conventional LPI and MPI  techniques. Often in LPI, the castings would have a tendency to bleed due to entrapment of excessive penetrant, hence proper cleaning of the penetrant are required.

 

ASME Sec VIII, DIV-1(Chapter UCI) is on cast iron pressure vessel. However welding is not greatly encouraged. Cast iron welding techniques are still more repair welding as of now.

 

Thanks.

 

Pradip Goswami,P.Eng

Senior Engineer/Specialist(Welding-Metallurgy)

Email-pradip.goswami@opg.com.

 

 

From: pgoswami@sympatico.ca [mailto:pgoswami@sympatico.ca]
Sent: Monday, April 19, 2010 10:42 AM
To: GOSWAMI Pradip -THERMAL
Subject: FW: [MW:4880] Welding of cast iron

 


 


Date: Mon, 19 Apr 2010 07:39:28 -0700
From: mkh_200@yahoo.com
Subject: [MW:4880] Welding of cast iron
To: materials-welding@googlegroups.com

What are the precautions before welding the ductile cast iron in pipe with Ø20?
Is there any NDT can applied after welding?
What is the applicable code for this welding??
 
SASA



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...