Yes, no need to purge when the accsses for back chip, but pickling passivation to be taken care.
V.Ravishanker
From: Ramesh Barot <rameshnbarot@yahoo.com>
To: Materials Welding <materials-welding@googlegroups.com>
Sent: Thu, 22 April, 2010 2:38:00 PM
Subject: [MW:4918] Purging
Dear All,
I have one doubt for purging of ss material. If we have inside excess for back chip then can we allow to do welding without purging in all cases?
Thanks,With Best Regards,
Ramesh Barot
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.