Dear gary,
 
now we are using the Lincoln Electric P223 flux , to weld the wind mill towers , but during welding we experience the following
1. uneven weld bead
2.excess reinforcement
3.bad cosmetic look
 
if decrease the amps to get good cosmetic look , during ut inspection the weld soundness fails. can you recommend a parameter for welding
 
Note:
 
the thickness range is 8mm to 20mm , we are practising square but welding .


 
On 3/5/10, Gary_Konarska@lincolnelectric.com.sg <Gary_Konarska@lincolnelectric.com.sg> wrote:

Depending on application:

Lincoln Electric 780 flux

Lincoln Electric P223 flux

Lincoln Electric 781 flux

Lincoln Electric SPX 80

Etc.


  From: "GERING, Erwin" [Erwin.GERING@airliquide.com]
  Sent: 03/05/2010 08:48 AM CET


  To: <materials-welding@googlegroups.com>
  Subject: [MW:4435] RE: 4421] Hispeed fluxes for SAW WELDING


Depending on application:

Oerlikon OP F55

Oerlikon Uniflux D1

Oerlikon OP 191

Etc…

 

With kind regards,

Erwin GERING

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens bcube bcube
Verzonden: donderdag 4 maart 2010 16:39
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:4421] Hispeed fluxes for SAW WELDING

 

Dear all,

 

Can any one sent me the details releated to the Hi speed fluxes used for SAW welding .

 

 

Reg,

RBG

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...