Wednesday, April 28, 2010

RE: [MW:4970] about boron content in SA 516 grade 70 plates

Dear Mr. Vikas

 

Boron requirement as an unspecified element  shall not exceed 0.0005 percent ( as per SA 941 under discussion chapter).

 

Regards

 

Prashanth Hegde

Head Quality

CICB-Chemicon Pvt. Ltd

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vikas Shah
Sent: Wednesday, April 28, 2010 11:48 AM
To: materials-welding@googlegroups.com
Subject: [MW:4969] about boron content in SA 516 grade 70 plates

 

Dear Sir

 

 

Is boron allowed in the SA516 grade 70 plates upto 0.0014%

 

 

 

Regards,

 

Vikas Dinesh Shah

 

Sanghavi Bothra Engineering Co. Pvt. Ltd.
56, Kika Street, Gulalwadi,
Mumbai – 400004. India.
Mobile: +91-9821532896
Tel: +91-22-40416200 / Fax: +91-22-23452161
Direct Line: +91-22-40416223
E-mail - vikas@sbecpl.com
Website: - www.sbecpl.com

 

Please consider the environment before printing this e-mail

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...