Dear Mr.Ramesh,
IBR(Indian Boiler Regulations) is code for boiler manufacturing and
applicable to any boiler manufactured and erection in India. All the
welding essential variables shall be as per IBR code only.
ASME Sec IX, is not applicable for IBR boilers.

Regards,

K.Ramalingeshwara Rao.

On Apr 27, 11:57 am, Ramesh Barot <rameshnba...@yahoo.com> wrote:
> Dear All,
>
> I am new for using IBR. I want to know in IBR use WPS can be qualified different way from ASME sec-9 or same as per SEC-9?
> Essential,Non essential and supplementary essential variables are same or different? and what about welder?
>  Thanks,
> With Best Regards,
> Ramesh Barot
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> Subscription settings:http://groups.google.com/group/materials-welding/subscribe?hl=en

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...