Best way would be to take down the actual thicknesses and hand over the data to your design engineer to reconcile...

--- On Fri, 23/4/10, omar fazni <ofazni@yahoo.com> wrote:

From: omar fazni <ofazni@yahoo.com>
Subject: [MW:4930] Corroded Beams (AISC)
To: materials-welding@googlegroups.com
Date: Friday, 23 April, 2010, 6:08 AM

Dear Members,

Does anyone has any experience of determining the tolerance of thickness reduction of a corroded beam (surface attack) with AISC code??

What happens is we have a W18x50 beam that is corroded all over one side of the web surface, after performing sandblast on the beam surface we found that the roughness is very high and already look like there are a lot of small pits.....

Using weld gauge after sandblasting the beam, we can measure some pits have reduced its thickness by more than 10%, about 1mm

Any response or shares will be appreciated

Tq & Regards
Omar Fazni


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...