Hi,
As per API 5L - 44th edition X85 grade is not there. For the CVN values refer 9.8.2.3 of API 5L 44 th edition.
K.Ramalingeshwara Rao.
On Wed, Apr 28, 2010 at 11:17 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
I heard that 44th edition of API 5L has 3 new grades X90, X100 and X120.what is X85? CVN is mandatory for all PSL2 pipes, refer para 6.2.5.2
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Tuesday, April 27, 2010 3:53 PM Subject: [MW:4966] API 5L X85 -CVN RequirementsGents,Pls tell me, what is the CVN (Longitudinal) Requirements for the API 5L X85 (19 mm thick) ?Thanks & Regards,K.Babu--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments