RE: [MW:4909] RE: 4421] Hispeed fluxes for SAW WELDING

For wind tower production Oerlikon has specially designed OP 139

 

With kind regards,

Erwin GERING

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens hakan sitem
Verzonden: dinsdag 20 april 2010 23:08
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:4908] RE: 4421] Hispeed fluxes for SAW WELDING

 

Regarding to SAW using during wind tower production, you can try Esab OK 1072 flux combination together with your wires which is already presented to be used in wind tower production.

Bu e-posta, Turkcell BlackBerry ile gönderilmiştir.


From: bcube bcube <bcubebcube@gmail.com>

Date: Tue, 20 Apr 2010 20:53:36 +0530

To: <materials-welding@googlegroups.com>

Subject: Re: [MW:4901] RE: 4421] Hispeed fluxes for SAW WELDING

 

Dear gary,

 

now we are using the Lincoln Electric P223 flux , to weld the wind mill towers , but during welding we experience the following

1. uneven weld bead

2.excess reinforcement

3.bad cosmetic look

 

if decrease the amps to get good cosmetic look , during ut inspection the weld soundness fails. can you recommend a parameter for welding

 

Note:

 

the thickness range is 8mm to 20mm , we are practising square but welding .


 

On 3/5/10, Gary_Konarska@lincolnelectric.com.sg <Gary_Konarska@lincolnelectric.com.sg> wrote:

Depending on application:

Lincoln Electric 780 flux

Lincoln Electric P223 flux

Lincoln Electric 781 flux

Lincoln Electric SPX 80

Etc.


  From: "GERING, Erwin" [Erwin.GERING@airliquide.com]
  Sent: 03/05/2010 08:48 AM CET


  To: <materials-welding@googlegroups.com>
  Subject: [MW:4435] RE: 4421] Hispeed fluxes for SAW WELDING

 

Depending on application:

Oerlikon OP F55

Oerlikon Uniflux D1

Oerlikon OP 191

Etc…

 

With kind regards,

Erwin GERING

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens bcube bcube
Verzonden: donderdag 4 maart 2010 16:39
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:4421] Hispeed fluxes for SAW WELDING

 

Dear all,

 

Can any one sent me the details releated to the Hi speed fluxes used for SAW welding .

 

 

Reg,

RBG

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...