Dear Phino,
You can try with the following.
- Shielding gas composition may be modified to: % of CO2 can be reduced to 0.5 and helium can be increased to 20-30%.
- Pulsed arc technique shall be used in order to avoid porosity and spatters.
Regards,
L. Prabhu kumar,
Sr. Principal Engineer,
Equipments & Materials Dept.,
Saipem India Projects Limited,
Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,
Mobile Ph. No.: +91 9003010978.
From:
Sent: Monday, April 26, 2010 5:16 PM
To:
Subject: [MW:4958] Super Duplex Welding
Dear All
We have problems for welding Super Duplex Nº 1.4410 (see attach of Base Material Certificate) with8 mm thickness.
The process is GMAW - MAG welding an use wire electrode AWS A5.9-06 : ER2594 (see attach of Wire electrode Certificate) and the shielding gas is Ar+20%He+2%CO2
The bead of first pass is OK, but the next pass (interpass) have lots of porosity, no penetration and Spatter.
Will bo control the temperature of interpass?
Will be change the wire electrode?
Thanks for help
Best Regards
Rui Fernandes Pinho
Divisão de Gases Industriais
Desenvolvimento de Aplicação de Gases
Linde Sogás, Lda.
Travessa Joaquim Dias Salgueiro, Nº 44
4470-416 Vila Nova da Telha,
Phone + 351 22 999 8380, Fax: + 351 22 996 4039
Mobile + 351 91 473 9197
rui.pinho@pt.linde-gas.com, www.linde.pt
--
To post to this group, send email to
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
| |
------------------------------------------------------------------------------------------------------------------------------------------------------------------- DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If you have received this communication in error, please notify us immediately by responding to this email and then delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete transmission of the information contained in this communication nor for any delay in its receipt. ------------------------------------------------------------------------------------------------------------------------------------------------------------------- |
Comments