dear syah,
                    The specification for A53  for Pipe, Steel, Black and Hot dipped, zinc coated, and seamless &  for A 106 Specification for seamless Carbon steel pipe for HIGH Temperature service....


 
On Mon, Mar 29, 2010 at 1:46 PM, Syahrian Zulfan <syahrian09@gmail.com> wrote:
Dear all,
 
can anyone advice me whether material Grd B53 and SA106-B is same? If yes what is differenting both of its
 
Rgds,
Syah

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.



--
Yadav Shiva Chelliya,
Inspection Engineer,
Doha Qatar,
+974-6166465

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...