Re: [MW:4555] Chemical composition check of clad weld

ASME BPV Sec IX doesn't specify (not mandatory) the depth at which chemical analysis to be carried, it is to be decided by the process designer based on corrosion rate and life of the component. 

On Sat, Mar 13, 2010 at 10:21 AM, sachin sankhe <sachin.sankhe@rediffmail.com> wrote:
Hi,

Do we have reference in any code on distance at which chemical compostion to be checked of weld clad from fusion line of base metal and weld metal?

Regards
Sachin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...