RE: [MW:4609] RE: 4606] RE: 4605] Welding consumable for SS 329

THE MATERIAL NO. IS 1.4460 WITH DIN DESIGNATION X 3 CrNiMoN 27 5 2.
 
THE ELECTRODE MAY BE USE 6810 MoKb and TIG RODS / MIG WIRES A6810Mo
 
THIS IS WITH REFERENCE TO UTP WELDING CONSUMABLES
 
AWS EN TESS Engros  Esab Elga Böhler Thyssen Soudokay UTP AWS EN AVESTA Metrode Selectarc Lincoln
A5.4/A5.11 EN1600   OK Cromarod FOX Thermanit     A5.4/A5.11 EN1600        
2209-15 22 9 3 N L B 2205 Bas 67.55 Duplex B CN 22/9 N-B 22/09 SOUDINOX S 4462 6808 MoKb 2209-15 22 9 3 N L B 2205 Bas 2205XKS Inox 2209 B Jungo Ziron 100 X

 
 
 
regards,
 
Farhan Talib


 
 



 
> From: mehmood.javed@fatima-group.com
> To: materials-welding@googlegroups.com
> Subject: [MW:4608] RE: 4606] RE: 4605] Welding consumable for SS 329
> Date: Thu, 25 Mar 2010 16:08:41 +0500
>
> UNS # is S32900
>
> Regards,
>
> Mahmood
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
> (Mumbai - PIPING)
> Sent: Thursday, March 25, 2010 1:18 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:4606] RE: 4605] Welding consumable for SS 329
>
> Pl specify UNS# or full specification, if it is for UNS# S32950/F52, you
> may use E/ER 2209
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Mehmood Javed
> Sent: Thursday, March 25, 2010 11:56 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:4605] Welding consumable for SS 329
>
>
> Dear All,
>
> Can somebody let me know the welding consumable specifications for SS
> 329 forging,
>
> Regards,
>
> Mahmood
>
>
>
> Filtered by Hosted Filtering
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribegooglegroups.com or reply to this email with
> the words "REMOVE ME" as the subject.
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.


Hotmail: Trusted email with Microsoft's powerful SPAM protection. Sign up now.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...