Wednesday, March 31, 2010

[MW:4644] Sub contract of weders(UW 26) (d)


Hi gents,
 
I have a query regarding the sub contact of welders.
Eg : I am working in company 'X'. I want to sub contract some welders from company 'Y'. If I qualify that welders as per my company welding pocedure (Company A procedures), is it equired to make a contract with that welders individually?. Or can I make a contract with that supply company?. UW 26 (d) says 'manufacturer may engage idividuals by contract as welder'.
 
Please povide a reply.

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...