Monday, March 29, 2010

[MW:4619] Need help regarding cutting blade material.

Dear all,
            i am working on the TMT bar cutting machines.There is shearing type cutting action . I found the frequect failure of. the cutting blade . i have selected S1 or K455 tool stell material for the same having hardness @ 56 to 58 HRC. CAn anybody Guide me / Suggest regarding the same.? 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...