Re: [MW:4581] EN10204 3.2 certification

Aarpee
 
Your defination for 3.2 certification is correct and you need to transmit the same defination to the base parent base material like plate,flange,pipe,fittings etc and again you to restrict this requirement upto pressure parts and metallic material
 
But you have to be careful while defineing the EN10204 standard in initial of the project by defining this requirement to pressure parts and attachment weld,based on criticality rating of the items of metallic parts,cost implication for implementation of  3.2 cert for non critical items and define the purchaser's intervention as 'witness'activiites for specific inspection.
 
This is verymuch required because EN10204 is sailent about purchaser involvement as witness or review and again this may applicable for non metallic componants .....
 
if you still need more info on this subject plz revert back.
 
Abhijit

--- On Thu, 18/3/10, Aarpee <ramprasad.chari@gmail.com> wrote:

From: Aarpee <ramprasad.chari@gmail.com>
Subject: [MW:4577] EN10204 3.2 certification
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Thursday, 18 March, 2010, 12:23 PM

Dear all,
My understanding about 3.2 certification is that only a 'component'
manufacturer can issue it with due endorsement by customer's
represenattive/customer's authorised representative.
CAN:
1 A pressure vessel manufacturer, who does only welding,NDT,Hydro
etc,issue 3.2 certificate??(he does this from components like
plates,pipes,flanges,fittings,fasteners,gaskets etc which can be
either in 3.1 certification or 3.2 certification)

2.A Piping Skid manufacturer and assembler, who also does
welding,NDT,Hydro,assembly,pneu test etc,issue a 3.2 certificate??(he
does this from components like
pipes,flanges,fittings,fasteners,gaskets,valves,meters,gauges,instruments,cables
etc which can be either with 3.1 certification or 3.2 certification)

Your input with experience on above shall be appreciated.
Regards
Aarpee

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...