hi all,
I'm encountering an interesting situation. My WPS progression is as follows
RP-up, Hot- up, fill & cap - downhill.
(dia-36" No of welders =2,Mat=API 5LX70, code = api1104,toughness and hardess requirements)
Now after root pass due to some unavoidable conditions the pipe has been rotated 90 degrees (12 o clock rotated to 3 o clock). Now considering one half
section of the pipe half portion is welded uphill with one welder and half downhill with the other welder
a) What should be the progression of next pass
b) How the welders must be allocated
c) What area (if required) must be selected for hardness and impact toughness testing.
hope the experts will comment
Sreejith Nair
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-