Thursday, March 25, 2010

[MW:4608] RE: 4606] RE: 4605] Welding consumable for SS 329

UNS # is S32900

Regards,

Mahmood

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
(Mumbai - PIPING)
Sent: Thursday, March 25, 2010 1:18 PM
To: materials-welding@googlegroups.com
Subject: [MW:4606] RE: 4605] Welding consumable for SS 329

Pl specify UNS# or full specification, if it is for UNS# S32950/F52, you
may use E/ER 2209

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Mehmood Javed
Sent: Thursday, March 25, 2010 11:56 AM
To: materials-welding@googlegroups.com
Subject: [MW:4605] Welding consumable for SS 329


Dear All,

Can somebody let me know the welding consumable specifications for SS
329 forging,

Regards,

Mahmood

Filtered by Hosted Filtering


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

To unsubscribe from this group, send email to
materials-welding+unsubscribegooglegroups.com or reply to this email with
the words "REMOVE ME" as the subject.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...