Tuesday, March 30, 2010

Re: [MW:4625] Weld A182 F91 TO SS 316

Use 309 grade filler metal but verify the FN first in order to avoid hot cracking.


  From: atilio vasquez [atiliovasquez16@hotmail.com]
  Sent: 28/03/2010 17:54 AST
  To: <materials-welding@googlegroups.com>
  Subject: [MW:4623] Weld A182 F91 TO SS 316



 Hi everyone, cuold somebody please let me know how weld  Branch SS 316 to ASTM A182 Gr. F91  (consumable and WPS).
Thanks in advance