Saturday, March 20, 2010

Re: [MW:4587] Piping welding Electrode Consumption

Dear Praveen,
   I have attached a table , i hope it will be useful to your requirement
with regards
N.Devan 

On Sat, Mar 20, 2010 at 9:38 AM, Praveen Kumar <praveenkumar.sek@gmail.com> wrote:
Dear all,
 
Can anybody give information to me regarding,
The Exact calculation of Piping welding Electrode Consumption
(for dia & sch/thkness wise)
 
If any formulas or tables pls assist me
 
 
Thanks & Regards,
 
Praveen Kumar
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.



--
Natarajan.Devan
Senior Welding Inspector
Al Furat Petroleum Co-Syria
Syria Shell Petroleum Development
Tel: 00963 11 6182103 Res
Mobile: 00963 933052385

INDIA: 0091 9840330143 Res.
Mobile: 0091 9884745254

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...