Re: [MW:4596] Piping welding Electrode Consumption

Dear Maringan Hutagalung,
Thank you for providing a better site, the calculator is simple but informative.
 
Regards
Chelliah M

On 22 March 2010 05:10, Maringan Hutagalung <maringan.hutagalung@gmail.com> wrote:
Dear Mr Kumar,

Please try a welding calculator on T-PUT Welding's web as your
practical tool to calculate filler metal consumptions for your welding
processes: http://www.t-put.com/english/634_ENG_HTML.htm

First you must to converse a diameter size become a length.

Enjoy the calculating..



Best regards,
Maringan Hutagalung


On 3/20/10, Praveen Kumar <praveenkumar.sek@gmail.com> wrote:
> Dear all,
>
> Can anybody give information to me regarding,
> The Exact calculation of Piping welding Electrode Consumption
> (for dia & sch/thkness wise)
>
> If any formulas or tables pls assist me
>
>
> Thanks & Regards,
>
> Praveen Kumar
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribegooglegroups.com or reply to this email with
> the words "REMOVE ME" as the subject.
>

--
Sent from my mobile device

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.



--
Chelliah M

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...