Dear all,

I need to make a PQR for 516 Gr 60N-HIC material for thickness ranging
from 10mm to 32mm with PWHT.
Please suggest me what additional tests are required for HIC(Hydrogen
Induced Cracking) material for the PQR along with Physical & Chemical
Tests.