Friday, October 16, 2009

[MW:3510] RE: 3477] Re: Grain size

As per ASME, fine austenitic grain size means austenitic grain size number of 5 or higher (finer).

 

Jignesh

 

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chaitanya Purohit
Sent: Sunday, October 11, 2009 07:36
To: materials-welding@googlegroups.com
Subject: [MW:3477] Re: Grain size

 

If the requirement is fine grain steel then the grain size shall be 7 or higher.



2009/10/10 Shashank Vagal <nach_sam@yahoo.com>

Senthil,
It should be in the MTR. But a fine grain size starts from 6 up.
Shashank

--- On Sat, 10/10/09, MNS <mn.senthilkumar@ymail.com> wrote:


From: MNS <mn.senthilkumar@ymail.com>
Subject: [MW:3469] Grain size
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, 10 October, 2009, 9:41 AM


May I know the Grain size of SA 516 Gr 70?


Thanks
Senthil


Now, send attachments up to 25MB with Yahoo! India Mail. Learn how

 




--
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...