Saturday, October 31, 2009

[MW:3570] RE: 3564] Re: acceptance crerteria of undercut

Hi dear

Thanks for your answer

But this is not my question according to iso 5817   we have not any short imperfection for thickness more than 3 mm.now what must I do ?

Best regards

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ankit gupta
Sent: Wednesday, October 28, 2009 3:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:3564] Re: acceptance crerteria of undercut

 

Slight intermittent undercut permitted provided

it does not form a sharp notch; depth

should not exceed @4 mm



WITH WARM REGARDS 
  ANKIT GUPTA 
    
Er@BHEL

--- On Wed, 10/28/09, Arjan van Vessum <vess_kiwi26@hotmail.com> wrote:


From: Arjan van Vessum <vess_kiwi26@hotmail.com>
Subject: [MW:3563] Re: acceptance crerteria of undercut
To: materials-welding@googlegroups.com
Date: Wednesday, October 28, 2009, 4:46 PM

Whats the wall tickness???
 
For criteria class C, check if h ≤0,1 t but max 0,5 mm...
If weld length is appr 100mm a 25mm discontinuity is allowed as per section 3.3 (EN ISO 5817)
 
greets,
 
Arjan van Vessum
 
 

 


Subject: [MW:3556] acceptance crerteria of undercut
Date: Wed, 28 Oct 2009 08:29:49 +0330
From: Samimi@mapnagenerator.com
To: materials-welding@googlegroups.com

Hi dear

Please let me know that according to iso 5817 rev: 2005 class C the undercut with 0.2mm depth and 24 mm length in Butt Weld and 100 mm length of our product is acceptable or not.if yes or no please explain exactly with detail.

 

Best regards

Alireza Samimi



__________ Information from ESET NOD32 Antivirus, version of virus signature database 4530 (20091021) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com



 

__________ Information from ESET NOD32 Antivirus, version of virus signature database 4530 (20091021) __________

 

The message was checked by ESET NOD32 Antivirus.

 

http://www.eset.com

 



__________ Information from ESET NOD32 Antivirus, version of virus signature database 4530 (20091021) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...