Hi!
We have recently organised a course on " Weld Defects Inspection and Quality
Assurance- WDIQA-2009" during 24-26th Aug, at Chennai. My question is: How
to get a defect free (closer to no defect-perfect) weld ? Group members can
try to list the precautions, procedures, etc, etc to be followed to obtain a
defect free weld (based on their experience). If we can compile all the
details, it will be an useful source of information for all of us.
Thank you,
Best Regards,
Vaidehi Ganesan.
=================================================================================================================
Dr. Vaidehi Ganesan,
Metallurgy and Materials Group,
Indira Gandhi Centre for Atomic Reseach,
Kalpakkam-603 102, India.
====================================================================================================================


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS