Saturday, October 31, 2009

[MW:3568] Re: acceptance crerteria of undercut

one classic rule of thumb,use your fingernail to feel the undercut.If it over the limit specified below(i.e unacceptable), you would feel the undercut.If not the fingernail(i.e undercut is in the acceptable range) will glide over the undercut smoothly.
 
Thanks
 
PGoswami
 

From: vess_kiwi26@hotmail.com
To: materials-welding@googlegroups.com
Subject: [MW:3563] Re: acceptance crerteria of undercut
Date: Wed, 28 Oct 2009 12:16:36 +0100

Whats the wall tickness???
 
For criteria class C, check if h ≤0,1 t but max 0,5 mm...
If weld length is appr 100mm a 25mm discontinuity is allowed as per section 3.3 (EN ISO 5817)
 
greets,
 
Arjan van Vessum
 
 

 

Subject: [MW:3556] acceptance crerteria of undercut
Date: Wed, 28 Oct 2009 08:29:49 +0330
From: Samimi@mapnagenerator.com
To: materials-welding@googlegroups.com

Hi dear

Please let me know that according to iso 5817 rev: 2005 class C the undercut with 0.2mm depth and 24 mm length in Butt Weld and 100 mm length of our product is acceptable or not.if yes or no please explain exactly with detail.

 

Best regards

Alireza Samimi



__________ Information from ESET NOD32 Antivirus, version of virus signature database 4530 (20091021) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com

</html
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...