[MW:3491] Porosity

Dear Friends;
 
We are constructing a pipeline with Semi - Automatic Orbital GTAW Welding System which is consist of cladded pipes. Pipe Material is API 5L X65 + Inconel 625 Overlay. We have completed nearly 20 km and when we were in a shortage of wire, we ordered a new batch of wire (Inconel 625). After receiving this wire we had porosity in all the joints especially below 3 oclock position.
 
Our habitats are in perfect condition, there is no any small wind inside.
Our gas (Argon) seems clear (up to this time we didnt face any problem).
We are cleaning the bevels with acetone.
 
Under the light of above explanations can you suggest me someways, how to avoid this porosity other than changing the wire.
 
Best regards
 
Ozgur
 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...