hai!
As for as piping is concern, we can't do SMAW welding in root pass. If you want to avoid backpurging in SS material, better to go for FCAW ,if the client has accepted.


 
On Mon, Oct 19, 2009 at 2:06 PM, ikaria73 <ikaria73@hotmail.com> wrote:

Minal Patel,
Lincoln Electric's STT process can be used as an alternative to open
root welding with stainless steel.  It is a GMAW process that with
proper training and technique can yield high productivity.

Regards,
TF

On Oct 15, 11:29 pm, "Minal Patel \(Sorge's Welding\)"
<mpa...@metalcare.com> wrote:
> Hi there,
>
> One of our manager wants to Develop WPS for SS which can utilize SMAW -root.
> I do not see it is common in SS welding. But there may be something can make
> us competitive against GTAW root.
>
> Does anybody have thought to share with me?
>
> Thanks in Advance..!
>
> Minal Patel
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---