[MW:3550] Re: Electrode for 17-4 PH cast steel

Dear Maringan,
If you have stock of 25/12 electrode you can use of it.
It is a superior electrode but costlier than the E630.
Muniyandi

On Tue, Oct 27, 2009 at 12:32 PM, Maringan Hutagalung <maringan.hutagalung@gmail.com> wrote:

Dear all,

Our customer as a pulp and paper mill service are repairing
a liner in a rotor housing, the material is a cast steel type 17-4PH.

For repair of some defect caused corrosion and abrasion wear, they
require an electrode AWS E630.

Does anyone can give an advice for other type of electrode to
substitute a E630 since
we don't have stock of it.

Thanks in advance


Maringan

--
Sent from my mobile device




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...